fracture

Crack Propagation in Bamboo's Hierarchical Cellular Structure

Submitted by Yang Lu on

Bamboo, as a natural hierarchical cellular material, exhibits remarkable mechanical properties including excellent flexibility and fracture toughness. As far as bamboo as a functionally graded bio-composite is concerned, the interactions of different constituents (bamboo fibers; parenchyma cells; and vessels.) alongside their corresponding interfacial areas with a developed crack should be of high significance.

The 2nd Sandia Fracture Challenge is here!

Submitted by blboyce on

update, 7/24/2014: The information packet ("SFC2-challenge-v5.ppt") is no longer attached to this post (iMechanica has a file size limit of 1 MB, so we can not attach the 6 MB file). IF YOU WOULD LIKE THE INFO PACKET, PLEASE E-MAIL ME, blboyce [at] sandia.gov and copy Dr. Sharlotte Kramer, slkrame [at] sandia.gov. If you have an older version of the information packet, please also e-mail for the newest (v5) info packet.

We intend to send the shear calibration data to all those whose e-mail address I have by August 1st (sorry for the delay!).

Call for abstracts: “Issues in computational modeling of damage, fracture and fragmentation of solid materials”

Submitted by Julian J. Rimoli on

As part of the 51st Annual Technical Meeting of the Society of Engineering Science (SES 2014) to be held at Purdue University, West Lafayette, IN, on October 1-3 2014, it is our pleasure to invite you to submit an abstract to the Symposium “Issues in computational modeling of damage, fracture and fragmentation of solid materials”.



What are the regular iteration steps of cohesive model based FEM for crack problems

Submitted by Wen Ye on

   Hi, 
         I'm now start to learn cohesive zone model based FEM for crack problems. According the a regular coehsize model (bilinear for example), the relative displacement and the cohesive stress are both unknwon, so iteration is required. My question is that what are the regular iteration steps?
 
Thanks. 

Symposium on Structure, Plasticity and Fracture of Inorganic Glasses in Paris

Submitted by Erik Bitzek on

Dear Colleagues,



we are organizing a symposium on Plasticity and Fracture in Inorganic Amorphous Materials at 



Condensed Matter in Paris 2014



to be held August 23 to 29, 2014. 



Your experimental or theoretical contributions are highly welcome. 

Please don't hesitate to contact us for more information.



The deadline for abstract submission is  April 1st 2014.



Looking forward to seeing you in Paris in August,