damage in composites

Composite crushing + CZONE application

Submitted by davidrbmelo on

Hello,


I am modelling a crushing simulation of a composite corrugated coupon using Abaqus/Explicit and CZONE Abaqus' application.

I am modeling the coupon using S4R elements and the impactor as a discrete rigid shell plate with a slow constant crushing speed or high initial velocity for quasi-static and dynamic crushing simulations respectively.

I am using Hashin damage in Abaqus/Explicit and Hashin and also Tsai-Wu on CZONE application.

Stochastic modeling of damage evolution in composites under environmental ageing

Submitted by rrahman on

Stochastic modeling of damage evolution in composites under environmental ageing

R. Rahman, A. Haque, Z. Wu


Journal of Engineering Mathematics

April 2013, Volume 79, Issue 1, pp 153-166

Abstract

Modelling of fiber failure in Abaqus

Submitted by parthchoksi on
Choose a channel featured in the header of iMechanica
Fiber Modelling of fiber failure in Abaqus ABAQUS, Fiber failure, failure criteria , Fiber Composite  , composite I am presently working on modelling of fiber failure inof a composite lamina on ABAQUS. After researching a lot, Even after researching a lot, I haven't been able to find a damage criteria which  can depict natural failure in of a fiber. I do not want to induce a crack in it and break it or put in a cohesive layer. I want to break it as it breaks naturally. 


Crack propagation in composites in presence of shear and pressure loads

Submitted by Roche on

Hi,

Assume that we have a composite structure consists of isotropic layers with a delamination (separation) between the layers. There is a compressive load

applying normal to layers surfaces and hence normal to the delamination (crack) which closes the delamination, and a shear load tangential to the crack surface.

the order of shear force is much smaller than the compressive load. can the delamination propagate du to this shear force?

Crack propagation in composites in presence of shear and pressure loads

Submitted by Roche on

Hi,

Assume that we have a composite structure consists of isotropic layers with
a delamination (separation) between the layers. There is a compressive load
applying normal to layers surfaces and hence normal to the
delamination (crack) which closes the delamination, and a shear load tangential to the
crack surface.

energy balance of surface-based cohesive of composite under impact in Absqus 6-10

Submitted by moustachiio on

Hi there! I am really new to Abaqus and I need to model a composite
laminated crash cone under impact to a flat solid wall (analytical
surface is used). I modelled a cone with a layers of conventional shell
elements with hashin failure criteria and surface-based cohesive
behaviour as interaction between layers representing the interface of
composite laminates. The model runs successfully but once I checked the
energy balance, the damage dissipation energy from the cohesive, it
turned out to be NEGATIVE (I think this is wrong).

Need recommendation of PhD courses

Submitted by BrianBak on
Choose a channel featured in the header of iMechanica
Hi 
I am a PhD. Student at Aalborg University at Department for Mechanical and Manufacturing Engineering in Denmark. In short my PhD project treats modeling delamination damage in laminated fibrous composite structures under quasi-static and cyclic loading. I am having a hard time finding good relevant PhD-courses so now I am turning to you to ask you if you can recommend any good courses falling under the following criteria:
  • Damage analysis of composite structures
  • Nonlinear FEM
  • Cohesive zone modeling