Superior Energy Dissipation by Ultrathin Semicrystalline Polymer Films Under Supersonic Microprojectile Impacts

Submitted by Ramathasan The… on

Distinct deformation mechanisms that emerge in nanoscale enable the nanostructured materials to exhibit outstanding specific mechanical properties. Here, we present superior microstructure- and strain-rate-dependent specific penetration energy (up to ∼3.8 MJ/kg) in semicrystalline poly(vinylidene fluoride-co-trifluoroethylene) (P(VDF-TrFE)) thin films subjected to high-velocity (100 m/s to 1 km/s) microprojectile (diameter: 9.2 μm) impacts.