computational material modeling

A unified mechanics theory-based model for temperature and strain rate dependent proportionality limit stress of mild steel

Submitted by cemalbasaran on

Strain rate and temperature dependent elastic limit of mild steel is investigated by developing a dislocation incipient motion-based proportionality limit stress model. Temperature effect on strain energy of an edge dislocation is modeled by using unified mechanics theory. Unified mechanics theory-based index, called thermodynamic state index, is used to model thermally assisted degradation of strain energy. Kinetic energy due to thermal vibrations is added to the kinetic energy of an accelerating dislocation.

A Postdoc Position Available in Computational Mechanics at KAUST

Submitted by harrison_hanfei on

The Division of Physical Sciences and Engineering at King Abdullah University of Science and Technology (KAUST) invites applications for a Postdoctoral fellow in Mechanical Engineering at the Composite and Heterogeneous Material Analysis and Simulation Laboratory (COHMAS, http://cohmas.kaust.edu.sa).

Job description