Structural Adhesive Bonding

Invitation to attend Mr. Ran Tao PhD defense at COHMAS lab, KAUST.

Submitted by Ahmed wagih on

 

Title:

Enhancing the bonding of CFRP adhesive bonding through laser-based surface preperation sterategies.

Abstract:

Carbon Fiber-Reinforced Polymers (CFRPs) have been widely applied in the aerospace and automotive industries to achieve unprecedented weight reductions. However, major challenges need to be solved in order to exploit their full potential, especially in the design of full composite primary structure, making then a vital part of the mobility and energy revolution.