On the mechanism and the length scales involved in the ductile fracture of a bulk metallic glass

Submitted by Parag Tandaiya on

A few years ago we published a paper in Acta Materialia elucidating the mechanism and length scales in the ductile fracture of bulk metallic glass through experiments and finite element simulations.

The link to the paper is here: 'On the mechanism and the length scales involved in the ductile fracture of a bulk metallic glass'.

I hope you enjoy reading the paper and find it useful in your research.