SLM Ti-6Al-4V Plastic Anisotropy
Tue, 2017-06-27 12:31 - kourousis
Cyclic Plasticity and Microstructure of As-built SLM Ti-6Al-4V: The Effect of Build Orientation
D. Agius, K.I. Kourousis, C. Wallbrink, T. Song
Materials Science & Engineering: A (2017) -- Free access to the full article available at: https://authors.elsevier.com/a/1VHXL_Ky~FZJ6H
»