Journal Club for March 2019: Fatigue of hydrogels

Submitted by Ruobing Bai on

Fatigue of hydrogels

Ruobing Bai (1,2), Zhigang Suo (1)

(1) John A. Paulson School of Engineering and Applied Sciences, Kavli Institute for Bionano Science and Technology, Harvard University

(2) Department of Mechanical and Civil Engineering, California Institute of Technology

 

The 2019 Franklin Institute Laureate Symposium honoring Dr. John A. Rogers held by Temple University, 9-12PM, April 10, 2019

Submitted by Jie. Yin on

 

Soft, Body-Integrated Microsystems Technologies

 

Franklin Institute Symposium honoring Dr. John A. Rogers 

Recipient of the 2019 Benjamin Franklin Medal in Materials Engineering

 

The 2019 Franklin Institute Laureate Symposium will be held at Temple University to honor Dr. John A. Rogers who received the Benjamin Franklin Medal in Materials Engineering for pioneering the engineering of flexible and stretchable electronic systems for e-health and exploratory neuroscience.

Criteria for selecting a reasonable and better measure of anisotropy

Submitted by Bin Liu on

Published in Physcal Review Letters: https://doi.org/10.1103/PhysRevLett.122.045502. Many materials are anisotropic. However, there is no widely accepted measure for characterizing the degree of elastic anisotropy. Here, assuming that the limiting case of extreme anisotropy should possess a positive semidefinite stiffness matrix, we propose three criteria to evaluate measures of anisotropy and show that the existing measures in the literature do not satisfy all of the proposed criteria.

Dynamics of periodically coupled parallel flexural elements: towards the modular design of metamaterial beams

Submitted by Ahmed Elbanna on

Periodic systems have attracted a lot of attention in science and engineering due to the existence of band gaps in their frequency spectra. Here, we study the flexural wave propagation in beams that are periodically connected in parallel and investigate how the contrast in the material and cross-sectional properties may affect the band structure of these systems and their dispersion properties.

PhD Positions in Multiscale Modeling of Materials Under Extreme Conditions

Submitted by Kmomeni on

PhD positions are open immediately in Advanced Hierarchical Materials by Design Labat Louisiana Tech Universityon multiscale modeling of materials under extreme conditions. This will be a collaborative project with MIT, Georgia Tech, and Idaho National Labthat is supported by Department of Energy.  The candidates must have earned a degree in Mechanical Engineering or related fields (applicants with a MSc will be given priority) and have a solid background in theoretical and computational mechanics.

WBDC 2019- International Workshop on Big Data and Computing

Submitted by Asst. Prof. Dr… on

WBDC 2019- International Workshop on Big Data and Computing

 

http://www.iwbdc.org/com.html

 

 

 

The conference flyer including the detail information  is attached.  

 

Contact Information:

Carrie Kit Tsui

Conference Managing Director

www.hksra.org

Flat/rm a 9/f Silvercorp International Tower 707-713 Nathan Road Mongkok, Hong Kong

Multiscale Design of Graphyne‐Based Materials for High‐Performance Separation Membranes

Submitted by Jingjie Yeo on

https://doi.org/10.1002/adma.201805665 Computational modeling and simulations play an integral role in the bottom‐up design and characterization of graph‐n‐yne materials. Here, the state of the art in modeling α‐, β‐, γ‐, δ‐, and 6,6,12‐graphyne nanosheets for synthesizing graph‐2‐yne materials and 3D architectures thereof is discussed. Different synthesis methods are described and a broad overview of computational characterizations of graph‐n‐yne's electrical, chemical, and thermal properties is provided.