Multiscale Design of Graphyne‐Based Materials for High‐Performance Separation Membranes

Submitted by Jingjie Yeo on

https://doi.org/10.1002/adma.201805665 Computational modeling and simulations play an integral role in the bottom‐up design and characterization of graph‐n‐yne materials. Here, the state of the art in modeling α‐, β‐, γ‐, δ‐, and 6,6,12‐graphyne nanosheets for synthesizing graph‐2‐yne materials and 3D architectures thereof is discussed. Different synthesis methods are described and a broad overview of computational characterizations of graph‐n‐yne's electrical, chemical, and thermal properties is provided.