Complex Ordered Patterns in Mechanical Instability Induced Geometrically Frustrated Triangular Cellular Structures

Submitted by Sung Hoon Kang on

We have studied how complex ordered patterns can appear from buckling-induced geometrically frustrated triangular cellular structures.

The paper is selected as the Physical Review Letters Editors' Suggestion and highlighted in Physics Synopsis as the link below.

http://journals.aps.org/prl/abstract/10.1103/PhysRevLett.112.098701