Source truncation and exhaustion: Insights from quantitative in-situ TEM tensile testing
‚Source truncation and exhaustion: Insights from quantitative in-situ
TEM tensile testing' by D. Kiener and A.M. Minor (http://dx.doi.org/10.1021/nl201890s).
‚Source truncation and exhaustion: Insights from quantitative in-situ
TEM tensile testing' by D. Kiener and A.M. Minor (http://dx.doi.org/10.1021/nl201890s).