Plasticity

Solid/Fluid Mechacnics

Submitted by yaronben on
Choose a channel featured in the header of iMechanica
Free Tags

Hi,

In my research i am trying to develop a new model for plastic deformation, and i suspect there is a strong similarity between

plasticity and turbulent flow !.

My question is: if there is workd done trying to apply Reynolds decomposition (Reynolds Stress) to the governing equations and solved plasticity problem in Solids?

thanks,

Yaron B.S.

Full time position with ANSYS Inc (Houston, TX)

Submitted by pepi on

ANSYS, Inc. has an immediate job opening in Houston, TX for a Technical Services Engineer.  This is a full time position.

The job entails providing advanced technical guidance on various aspects of computational Structural Mechanics to clients in industry and academia.

Full scholarships available at European Commission funded workshop on physically based material modeling

Submitted by Tuncay Yalcinkaya on

European Commission' s JRC (Joint Research Centre) is organizing a workshop on physics based modeling of material properties and experimental observations in collaboration with METU (Middle East Technical University). The workshop will be held in Ankara on 22-23 October 2012.

The Workshop will include lectures by keynote speakers: W. Curtin, F. Dunne, L. Malerba, J-F Molinari, A. Needleman and B. Svendsen, and presentations by participants (oral or posters).

PhD Students/Post-doctoral Associates- North Carolina State University

Submitted by zikry on

Our group at North Carolina State University is hiring PhD students and Post-doctoral Associates in the areas of multiscale modeling, computational mechanics, fracture, and plasticity.

Interested parties should email  zikry [at] ncsu.edu, and send a cv with a few representative publications.

MA Zikry 

Stress Relaxation

Submitted by Amit Pandey on

2012-07-10

I would like to seek comments on : Room temperature stress relaxation and governing mechanisms that contribute to the plasticity that occurs during this process. As, most of the available work on relaxation is done at elevated temperatures.



Please check more on this thread by hari@



node/12687



 I have also attach papers by Prof Hart and Prof Krempl that did throw some light on this particular subject.

stress relaxation- doubt

Submitted by hariharan on

Attached herewith a classical paper by Hart on introducing a concept of constant hardness curves refuting that absolute strain should not be considered as a state variable.

 

The interesting part is he uses a stress relaxation test to prove the same. Stress relaxation test, here refers to a tensile test, where the test is stopped after say certain amount of plastic deformation. The stress drops a little, but the total strain is constant. However, it is argued that there is a small inelastic deformation, which is the cause of this load or stress drop.