in-situ Young's moduli of the constitutive layers in a multilayer systems (e.g. thin films, SOFCs, TBCs etc.)

Submitted by Amit Pandey on

 

This recent article present an improved methodology to calculate in-situ Young's moduli of the constitutive layers in a multilayer systems (e.g. thin films, SOFCs, TBCs etc.)

Pandey, A., Shyam, A., Liu, Z., & Goettler, R. (2014). In-situ Young’s Moduli of the Constitutive Layers in a Solid Oxide Fuel Cell. Journal of Power Sources.

 

http://www.sciencedirect.com/science/article/pii/S0378775314015341 

 

Highlights

in-situ Young's moduli of the constitutive layers in a multilayer systems (e.g. thin films, SOFCs, TBCs etc.)

Submitted by Amit Pandey on

 

This recent article presents an improved methodology to calculate in-situ Young's moduli of the constitutive layers in a multilayer systems (e.g. thin films, SOFCs, TBCs etc.)

 

Amit Pandey, Amit Shyam, Zhien Liu, Richard Goettler, In-situ Young's moduli of the constitutive layers in a solid oxide fuel cell, Journal of Power Sources, Volume 273, 1 January 2015, Pages 522-529

 

http://www.sciencedirect.com/science/article/pii/S0378775314015341 

TMS- 2015 CALL FOR ABSTRACT (Symposium on HIGH TEMPERATURE SYSTEMS FOR ENERGY CONVERSION AND STORAGE)

Submitted by Amit Pandey on

HIGH
TEMPERATURE SYSTEMS FOR ENERGY CONVERSION AND STORAGE

 

TMS Division: Functional Material Division (FMD
formerly known as EMPMD)

FMD sub-committee: Energy Conversion and Storage

 

Organizers:

Post-doc in micromechanical testing at Oak Ridge National Laboratory

Submitted by Amit Shyam on

We have an immediate opening for a post-doctoral candidate in the area of micromechanical testing within the Mechanical Properties and Mechanics group at ORNL.  Please see the attached file for further details.  If you are interested in the position, please apply online at:

https://www2.orau.gov/ORNL_POST/.