Designing ultratough single-network hydrogels with centimeter-scale fractocohesive lengths via inelastic crack blunting
Jie Ma, Xizhe Zhang, Daochen Yin, Yijie Cai, Zihang Shen, Zhi Sheng, Jiabao Bai, Shaoxing Qu, Shuze Zhu*, Zheng Jia*, Designing ultratough single-network hydrogels with centimeter-scale fractocohesive lengths via inelastic crack blunting, Advanced Materials, 2311795, 2024