mechanical metamaterials; mechanical coupling; micropolar elasticity; non-centrosymmetry

Axial-bending mechanical coupling

Submitted by Joshua on

We discovered a novel mechanical coupling effect โ€“ axial-bending coupling. Unlike Poisson, axial-shear, and axial-twisting coupling effects, this axial-bending coupling occurs at a non-centrosymmetric square lattice.

For more information, you can check this paper:
https://www.sciencedirect.com/science/article/pii/S0264127522001538