Enhancement of hydroxyapatite dissolution through structure modification by Krypton ion irradiation

Submitted by Dr. Hanaor - D… on

Heavy ion irradiation can be used to modify the atomic structure of a material and improve its dissolution characteristics as shown here. This has implication for the design of bioceramics

 