Modeling SMA-enabled soft deployable structures for kirigami/origami reflectors

Submitted by Jinxiong Zhou on

The synergic combination of smart soft composites with kirigami/origami principles leads to self-deployable systems. To date, the development of soft deployable structures has largely been an empirical process. Focusing on the recently developed shape memory alloy (SMA)-based soft deployable structures, this paper describes an analytical model and a finite element (FE) numerical scheme to investigate deformation and deployment performance of this system.