Wallner lines, crack velocity and mechanisms of fracture in a brittle bulk metallic glass

Submitted by Parag Tandaiya on

A few years ago, we observed Wallner Lines on the fracture surface of a brittle Bulk Metallic Glass and explained the process of formation of nanocorrugations on the fracture surface.

We published our research in Acta Materialia in the paper: 'Wallner lines, crack velocity and mechanisms of fracture in a brittle bulk metallic glass'.

I hope the experimental fracture mechanicians would particularly enjoy reading this paper and find it useful in their research.