Improved formulas of extensional and bending stiffnesses of rectangular nanorods

Submitted by Ajeet Kumar on

Improved formulas of extensional and bending stiffnesses of isotropic rectangular nanorods are derived. These formulas reduce to the existing widely used formulas for a special choice of material parameters, i.e., when the surface Poisson's ratio and the bulk Poisson's ratio match thus highlighting the limitation of the existing formulas.

A variant of Irving-Kirkwood-Noll formulation for one-dimensional nanostructures

Submitted by Ajeet Kumar on

We present a one-dimensional variant of the Irving-Kirkwood-Noll procedure to derive microscopic expressions of internal contact force and moment in one-dimensional nanostructures. We show that these expressions must contain both the potential and kinetic parts: just the potential part does not yield meaningful continuum results. We further specialize these expressions for helically repeating one-dimensional nanostructures for their extension, torsion and bending deformation. As the Irving-Kirkwood-Noll procedure does not yield expressions of stiffnesses, we resort to a thermodynamic equilibrium approach to first obtain the Helmholtz free energy of the supercell of helically repeating nanostructures. We then obtain expressions of axial force, twisting moment, bending moment and the associated stiffnesses by taking the first and second derivatives of the Helmholtz free energy with respect to conjugate strain measures. The derived expressions are used in finite temperature molecular dynamics simulation to study extension, torsion and bending of single-walled carbon nanotubes and their buckling.
The article will soon appear in the Mathematics and Mechanics of Solids. The same can be accessed at the following link: https://www.researchgate.net/publication/337873624_Microscopic_definiti…

Effect of surface elasticity on extensional and torsional stiffnesses of isotropic circular nanorods

Submitted by Ajeet Kumar on

We present a continuum formulation to obtain simple expressions demonstrating the effects of surface residual stress and surface elastic constants on extensional and torsional stiffnesses of isotropic circular nanorods. Unlike the case of rectangular nanorods, we show that the stiffnesses of circular nanorods also depend on surface residual stress components. This is attributed to non-zero surface curvature inherent in circular nanorods.