Magneto-Mechanical System to Reproduce and Quantify Complex Strain Patterns in Biological Materials

Submitted by Daniel Garcia-โ€ฆ on

Based on magneto-active polymers, we provide a non-invasive and real-time control methodology to impose complex mechanical forces on biological systems. The device is conceptualised to be suitable for any traditional microscope! See scheme:

We allow for reproducing complex mechanical processes by simulating a set of local strain patterns occurring in real scenarios. We demonstrated this by simulating strain distribution occurring within the brain tissue during a head impact (Knutsen et al., 2020 #BMphi).