Using ABAQUS subroutine (UMAT,VUMAT) to modeling FGM plate

Submitted by mahmoud.k.e on

Hello every body

I am working on modeling FGM plate in abaqus6.8,i know that it's possible to modeling FGP by using UMAT subroutine for definig variation of material's properties,but i don't know how can i use this subroutine,could you tell me please?



Hello,





here are a few links on spatial variation of material properties





1) get this PhD thesis:



DYNAMIC STRESS INTENSITY FACTORS

FOR HOMOGENEOUS AND NONHOMOGENEOUS MATERIALS

USING THE INTERACTION INTEGRAL METHOD

BY

SEONG HYEOK SONG

THESIS

Submitted in partial fulfillment of the requirements

for the degree of Master of Science in Civil Engineering

in the Graduate College of the

University of Illinois at Urbana-Champaign, 2003





The code appears also in

Buttlar, W., Paulino, G., and Song, S. (2006). ”Application of Graded Finite Elements for Asphalt Pavements.” J. Eng. Mech., 132(3), 240–249.

Application of Graded Finite Elements for Asphalt Pavements





2) http://www.imechanica.org/node/9485

Varying material properties spatially in ABAQUS





3) http://www.imechanica.org/node/614

Functionally Graded Materials





4) SIMULIA Learning Community

http://www.3ds.com/products-services/simulia/academics/simulia-learning…

Defining Depth Dependent Material Properties in Abaqus

by: Jessica NICHOLSON, 2013-10-17





5) http://paulino.cee.illinois.edu/software.html

Development of user subroutines in commercial software (UMAT and UEL in ABAQUS)





6) a former reply in the ABAQUS mailing list

http://groups.yahoo.com/neo/groups/Abaqus/info



----------------------------------------------------

Changing material property over coordinates



You should be able to define your elastic modulus values as a tabular

function of a field variable (set the number of field variables to "1"

when defining an elastic material in the "Edit Material" dialog box).

In this case, the field variable value will correspond to your

Y-coordinate. Unfortunately, ABAQUS/CAE doesn't currently support the

definition of predefined field variables (even though it has tools to

define discrete and analytical fields which can be used in interaction

and load definitions). So, you'll need to edit the input file to add a

*INITIAL CONDITIONS,TYPE=FIELD,VARIABLE=1 section and/or a

*FIELD,VARIABLE=1 section to actually define the field variable values.

Alternatively, you can use the UFIELD subroutine (this might actually

be easier, since the coordinates of the nodes are passed into the

subroutine, and all you'll have to do is set FIELD(NSECPT,1) = COORDS(2)).



Regards,

Dave



-------------------------

Dave Lindeman

Lead Research Specialist

3M Company

3M Center 235-3F-08

St. Paul, MN 55144

651-733-6383



S.M.Ali Tasaloti wrote:

>

>

> Hello to all,

> Maybe my question is easy but I didn't find any answer for it. I want

> for example to change the young modulus of material linearly over

> y-coordinate of the 2D model.

----------------------------------------



Regards



Frank

------------------------------------------
Ruhr-University
Bochum
Germany