finally with my colleagues G.Ferrari and I.Lelli I finished the simulation work about friction stir welding...We are very excited because the simulation gave us the expected results. The maximum temperature does not exceed the melting of the material, the pattern of isotermee is congruent with the results shown in the literature and various checks seem to justify the work done ...so now we are waiting the verdict of the professor with fingers crossed...

fabrizio leone

I am working on friction stir welding process in that i have to move
tool shape heat source in plate to find out temperature distribution in
plate . I have make circular shape heat source on the surface of the
plate but i want to make cylindrical shape pin as a heat source in that.
presenyly i am using dflux subroutine pls help me.

that is my soubroutine 

  SUBROUTINE DFLUX(FLUX,SOL,KSTEP,KINC,TIME,NOEL,NPT,COORDS,JLTYP,

     1             TEMP,PRESS,SNAME)

        

          INCLUDE 'ABA_PARAM.INC'

        

          DIMENSION FLUX(2),TIME(2),COORDS(3)

          CHARACTER*80 SNAME

          integer DZ

         REAL V,Q1,Q2,Q3,CX,CY,DX,DY,r

            

            

              V = 0.002

              Q1 = 4640014.831

              Q2 = 2000000

              Q3 = 1202051

              CX = 0.05

              CY = V*TIME(2)

              

          

              DX = COORDS(1)-CX

             DY = COORDS(2)-CY

             

              r = sqrt(DX**2 + DY**2)

!            

          IF(COORDS(3).LT.2e-04) THEN

          

            IF ((r.ge.0.004).AND.(r.le.0.0125))THEN

                  flux(1)=Q1*r

            ENDIF

          ENDIF

          

          IF((COORDS(3).GT.2e-04).AND.(COORDS(3).LT.41E-04)) THEN

                IF ((r.ge.0.0039).AND.(r.le.0.0040))THEN

                    flux(1)=Q2*r

                ENDIF

          ENDIF

          IF((COORDS(3).GT.41E-04).AND.(COORDS(3).LT.43E-04)) THEN

              IF (r.le.0.0040)THEN

                    flux(1)=Q3*r

                ENDIF

          ENDIF

                     



             RETURN

             END

i am able to restrict pin to some length

 

Wed, 09/19/2012 - 06:22 Permalink