Soft network materials with isotropic negative Poisson's ratios over large strains

Submitted by Yihui Zhang on

Auxetic materials with negative Poisson's ratios have important applications across a broad range of engineering areas, such as biomedical devices, aerospace engineering and automotive engineering. A variety of design strategies have been developed to achieve artificial auxetic materials with controllable responses in the Poisson's ratio. The development of designs that can offer isotropic negative Poisson's ratios over large strains can open up new opportunities in emerging biomedical applications, which, however, remains a challenge.

Shape memory effect and pseudoelasticity behavior in tetragonal zirconia polycrystals: A phase field study

Submitted by mohsenzaeem on

Shape memory effect and pseudoelasticity behavior in tetragonal zirconia polycrystals: A phase field study, International Journal of Plasticity 60 (2014) 71–86. Martensitic tetragonal-to-monoclinic transformation in zirconia is a ‘‘double-edged sword’’, enabling transformation toughening or shape memory effects in favorable cases, but also cracks and phase degradation in undesirable scenarios.