Johsnon-cook model

Johsnon-cook model parameter determination

Submitted by psarunirtt on

Hello All!!!

 I am Arun, Master degree student in South Korea.

 My research field is : High strain rate experiemnts

 I did High speed tensile test for aluminium alloy at four different speeds (1m/s, 5m/s, 10m/s and 15m/s)

 I also did high temp tensile test for aluminium alloy at room temperature, 100 C, 250C

 Now i have the stress Vs Strain curve for High speed tensile test and high temperature test

 But, i don't know how to determine Johnson-Cook model parameter from the experimental results