1D Plasticity - Isotropic hardening, tutorial with examples.

For those who may be interested,

 I have put together a paper describing 1D plasticity for a variety of cases of isotropic hardening.  The material is not new, but hopefully it is written with enough detail that it will help beginners learn some basics of computational plasticity.  The notation and material closely follows "Computational Inelasticity" written by Simo and Hughes.