Skip to main content

hyperelasticity

Multi-phase hyperelasticity with interface energy effect

Submitted by Zhuping Huang on

Recently, J. Wang, L. Sun and I have formulated some ideas about the effective properties of heterogeneous materials with surface/interface energy effect, which are shown in the attached file.

Papers in the attached file can be viewed as a two-part paper, called “Multi-phase hyperelasticity with interface energy effect” if it is standalone. Part one of this topic is covered in “A theory of hyperelasticity of multi-phase media with surface/interface energy effect”, which provides theoretical background. Part two is covered in “Size-dependent effective properties of a heterogeneous material with interface energy effect: from finite deformation theory to infinitesimal strain analysis”, with more emphasis on application.