Micro-cantilever beam fracture

Size effects and failure regimes in notched micro-cantilever beam fracture

Submitted by Parag Tandaiya on

Notched micro-cantilever beam fracture (MCF) experiments are increasingly being used to measure fracture toughness of materials at the micro-scale and draw conclusions about size-effects in them. In our recent paper published in Acta Materialia, 'Size effects and failure regimes in notched micro-cantilever beam fracture', we elucidate the failure regimes in MCF experiments and discuss the conditions for validity of MCF tests.