A new planner BCN lateral heterostructure with outstanding strength and defect-mediated superior semiconducting to conducting properties

Submitted by mohsenzaeem on

Motivated by the recent synthesis of boron-carbon-nitride (BCN) monolayers with different atomic compositions, we propose a novel planar BCN lateral heterostructure with a combination of graphene and hexagonal boron nitride (h-BN) counterparts. Density functional theory (DFT) and classical molecular dynamics (CMD) simulations are integrated to examine the effects of defects (vacancy and Stone-Wales (SW) defects) and temperature on the physical properties of the BCN heterostructure.