Si/Ge (111) semicoherent interfaces: Responses to an in-plane shear and interactions with lattice dislocations Submitted by Shuozhi Xu on Tue, 08/25/2020 - 02:35 research semicoherent interfaces multiscale modeling https://doi.org/10.1002/pssb.202000274 Abstract Read more about Si/Ge (111) semicoherent interfaces: Responses to an in-plane shear and interactions with lattice dislocationsLog in to post comments1823 views