Unraveling the molecular mechanisms of thermo-responsive properties of silk-elastin-like proteins by integrating multiscale modeling and experiment
http://dx.doi.org/10.1039/C8TB00819A
Fresh in 2018 Journal of Materials Chemistry B HOT Papers! We present integrative experimental and computational understanding of the thermal response in adaptive hydrogels tailor-made from silk-elastin-like proteins that are tunable and responsive to multiple simultaneous external stimuli.