Skip to main content

uhmwpe

Fatigue crack propagation

Submitted by Lazuardi Pujilaksono on
Choose a channel featured in the header of iMechanica

Hi, I'm trying to perform a supposedly-simple experiment on fatigue crack propagation of UHMWPE. I use a compact-tension specimen on a servopulser hidraulic testing machine. I will try to do the experiment on a fix Pmax with a varied force ratio (R) from 0.1 to 0.5. I'm having trouble in deciding the maximum force Pmax. How does one decide the amount of force applied for FCP testing? Calculation steps and so on.