Nonlinear Anisotropic Viscoelasticity
In this paper we revisit the mathematical foundations of nonlinear viscoelasticity.
In this paper we revisit the mathematical foundations of nonlinear viscoelasticity.
A central tool of nonlinear anelasticity is the multiplicative decomposition of the deformation tensor that assumes that the deformation gradient can be decomposed as a product of an elastic and an anelastic tensor. It is usually justified by the existence of an intermediate configuration. Yet, this configuration cannot exist in Euclidean space, in general, and the mathematical basis for this assumption is on unsatisfactory ground.