Submitted by konanur on

I am trying to use material model 58 of ls dyna to simulate a drop tower test on a carbon fibre epoxy composite. However i am getting poor simulation results with very high eroded internal energy values for composite.  My parameters are as follows

 

Hollow composite cylinder (with quad shell elements) of thickness 5mm with a mass of about 120g.

Impactor of weight 82 kg with impact vel of 6 m/s (direction along the longitudinal of composite cylinder)

material model in ls dyna : MAT 58

Currently am using Contact Auto single surface. Can i use any other contact algorithm and why?

Also how do i determine the optimum value of ERODS in MAT 58?

Answers to these queries and other suggestions are solicited

regards

Suhas