Skip to main content

bauchinger effect

Submitted by danielteruna on

Hi! all

I have conducted several test of steel plate under cyclic load in order to get hysteretic cuve. some specimens showed a significant differences between tension and compression load. I read from texbook about this phenomena and it say because of bauschinger effect. Iam wondering why the diffrences to large and sometimes more than 50%. I am very appreciate if some one can explain about this problem.

regards

danile