HI ALL
Actually I am a Student of 2 year M. Tech. studying in S. V. National Institute of Technology, Surat My name is Zoeb K Lakdawala. My topic for disseration is 'Implemenation of Fracture Mechanics on Pressure Vessels". In my disseration I want to develop a code on fracture mechanics and compare it with standard Packages like ANSYS & ABAQUS.
Actually In this project work i also wanted to conduct fracture toughness test using ASTM E - 1820 for that i have prepared the specimen as per ASTM E - 399( For measuring Stress Intensity Factor) & ASTM E - 1820(For Determination of J-R curve) using material SA 516 GR 70 but the major hindrence while reading the ASTM E - 1820 is that i how can i measure dm = total measured load-line displacement.
I will be most thankful to you if you give me suggestion regarding that
Forums
Hello zoeb I am also
Hello zoeb
I am also working with fracture toughness experiment. There are many possibilities to measure the load-displacement curve.
We used the split Hopkinson pressure bar for dynamic impact and measured the load-displacement values from classical theory.
So it depends on insturement you are employing if you want to measure the load-displacement curves experimentally.
I read Prof. C.T. Sun's paper (J.L. Tsai, C. Guo, and C.T. Sun, โDynamic Delamination Fracture Toughness in Unidirectional
Polymeric Composites,โ Composites Science and Technology, Vol. 61, 2001, pp. 87-94) and used crack gage to detect the crack
initiation time.
In reply to Hello zoeb I am also by syn1003
thanks
Thanks Chul JIn syn
for your reply can you suggest me some reference books for measuring the same
regards
Zoeb Lakdawala
Plane-Strain Fracture Toughness
Hi all
I am planning to estimate plane-strain fracture
toughness of my material based on E1820 with using one sample. There
are two procedurs in this standrad: 1) the basic method & 2) the
resistance curve method. I am looking for J1c and not R-curve. Do you
know if it is possible to use resistance curve method to get the
plane-strain facture toughness?
Thank you.
SEK