Abstract: In the present paper we investigate indentation of a power-law axisymmetric rigid probe in adhesive contact with a "thin layer" laying on a rigid foundation for both frictionless unbounded and bounded compressible cases. The investigation relies on the "thin layer" assumption proposed by Johnson, i.e. the layer thickness being much smaller than the radius of the contact area, and it makes use of the previous solutions proposed by Jaffar and Barber for the adhesiveless case. We give analytical predictions of the loading curves and provide indentation, load and contact radius at the pull-off. It is shown that the adhesive behavior is strongly affected by the indenter shape; nevertheless below a critical thickness of the layer (typically below 1 µm) the theoretical strength of the material is reached which in contrast with the Hertzian case, which has been shown to be insensitive to the layer thickness. Two cases are investigated, namely, the case of a free layer and the case of a compressible confined layer, the latter being more "efficient", as, due to Poisson effects, the same detachment force is reached with a smaller contact area. It is suggested that high sensitive micro-/nanoindentation tests may be performed using probes with different power law profiles for characterization of adhesive and elastic properties of micro-/nanolayers.
I see this post is gathering a lot of unexpected attention... Are adhesive properties of micro/nanolayers a hot topic for many of you? Discussions are welcome as we are also thinking at some further developments...
This is your first paper as a single author, congratulations!
It is always nice to see your former students to develop their own career path, and become independent.
And also, with this very nice and impressibly clean analysis.
I think if you dedicate more attention to this problem, you will find application in nano-thin-films testing.
In reply to This is your first paper as a single author, congratulations! by Mike Ciavarella
Thanks, I have to say I had a
Thanks, I have to say I had a good advisor!!!
Interested in adhesion of thin coatings?
I see this post is gathering a lot of unexpected attention... Are adhesive properties of micro/nanolayers a hot topic for many of you? Discussions are welcome as we are also thinking at some further developments...
final version published with some errata corrige
There were some wrong prefactors, if I understand well, which were fixed in final version
See http://casopisi.junis.ni.ac.rs/index.php/FUMechEng/article/view/3588
In reply to final version published with some errata corrige by Mike Ciavarella
I have update the final
I have update the final version also on imechanica (see PDF attached).