Giant voltage-induced deformation in dielectric elastomers near the verge of snap-through instability
Dielectric elastomers are capable of large voltage-induced deformation, but achieving
such large deformation in practice has been a major challenge due to electromechanical
instability and electric breakdown. The complex nonlinear behavior suggests an important
opportunity: electromechanical instability can be harnessed to achieve giant voltage-induced
deformation.
We introduce the following principle of operation: place a dielectric elastomer
near the verge of snap-through instability, trigger the instability with voltage, and bend the
snap-through path to avert electric breakdown. We demonstrate this principle of operation
with a commonly used experimental setup—a dielectric membrane mounted on a chamber of air.
We use a computational model to analyze inhomogeneous deformation and map out bifurcation
diagrams to guide the experiment. With suitable values of the parameters, we obtain giant
voltage-induced expansion of area by 1692%, far beyond the largest value reported in the
literature.
Attachment | Size |
---|---|
![]() | 1.59 MB |
![]() | 41.12 KB |
![]() | 63.22 KB |
- Tiefeng Li's blog
- Log in or register to post comments
- 5490 reads

Comments
great work!
great work!