Submitted by Anonymous (not verified) on Sun, 05/17/2009 - 18:04 education I want to know about the basics of stroh fromulation and its application in Piezoelectric material.I didn't find the basic lecture notes or the material regarding that on the internet. kuldeep sharma Zhigang Suo Re: Stroh formulation The following paper contains a basic description of the Stroh formulation, along with some references. Z. Suo, C.-M. Kuo, D.M. Barnett and J.R. Willis,"Fracture mechanics for piezoelectric ceramics," J. Mech. Phys. Solids40,739-765 (1992). Log in to post comments Wed, 05/20/2009 - 02:08 Permalink kuldeep (not verified) Re:stroh formulation Sir, Thanks for the Paper "Fracture mechanics for piezoelectric ceramics,". kuldeep sharma Log in to post comments Thu, 05/21/2009 - 02:20 Permalink Log in to post comments5008 views
Zhigang Suo Re: Stroh formulation The following paper contains a basic description of the Stroh formulation, along with some references. Z. Suo, C.-M. Kuo, D.M. Barnett and J.R. Willis,"Fracture mechanics for piezoelectric ceramics," J. Mech. Phys. Solids40,739-765 (1992). Log in to post comments Wed, 05/20/2009 - 02:08 Permalink
kuldeep (not verified) Re:stroh formulation Sir, Thanks for the Paper "Fracture mechanics for piezoelectric ceramics,". kuldeep sharma Log in to post comments Thu, 05/21/2009 - 02:20 Permalink
Re: Stroh formulation
The following paper contains a basic description of the Stroh formulation, along with some references.
Z. Suo, C.-M. Kuo, D.M. Barnett and J.R. Willis,"Fracture mechanics for piezoelectric ceramics," J. Mech. Phys. Solids40,739-765 (1992).
Re:stroh formulation
Sir,
Thanks for the Paper "Fracture mechanics for piezoelectric ceramics,".