Hi all,
I 'm interested in finding a complete seachable database on carbon/epoxy orthotropic prepreg [properties and values]. Those values are needed to be inputted into my finite element program for my thesis. One of those materials which i'm trying to find is the MR50/LTM25 as well as several others.
Any suggestions would be great
Thanks
Kind regards,
Ee Lian
Hello Lian You can find
Hello Lian
You can find some reference database for composite materials.
The website adress is
http://www.niar.twsu.edu/agate/Documents/
It maybe different material you are finding but it will be very good references.
C.J.Syn
Thanks C.J. Syn Really
Thanks C.J. Syn
Really appreciate it