Various outcomes of slip-coherent twin boundary depending on the stress state and slip geometry (during the growth of a microstructurally short crack)
Various outcomes of slip-coherent twin boundary depending on the stress state and slip geometry (during the growth of a microstructurally short crack)
Comparison of experimental literature on nanotwinned NiCo alloys and pure Cu – a correlation between the twin lamellar thickness (and/or spacing) and the damage trends has been noted.
Fatigue crack growth in presence of nano-twins with coherent Σ3 boundaries.