Hi
I am looking for the
experimental method to determine the parameters (D1, D2, D3, D4, D5) in Johnson
Cook damage criterion for steel St52 & St14. Please help me if you have any
sources relative this. Thank you.
Forums
Hi
I am looking for the
experimental method to determine the parameters (D1, D2, D3, D4, D5) in Johnson
Cook damage criterion for steel St52 & St14. Please help me if you have any
sources relative this. Thank you.
is explained in this paper
Hope this helps
Quasi-static and dynamic loading responses and constitutive modeling of titanium alloys Original Research Article
International Journal of Plasticity, Volume 20, Issue 12, December 2004, Pages 2233-2248
Akhtar S. Khan, Yeong Sung Suh, Rehan Kazmi
described in detail in Johnson's paper
the experimental method is described in detail in the original paper. I can e-mail you the paper if you need.
Hi I am looking for the
Hi
I am looking for the experimental method to determine the parameters ductile damage criterion for steel St52 & St14. Please help me if you have any sources relative this. Thank you.