Modeling the COnstitutive Response of Metals Under Complex Loading - 2012

Submitted by SIMULIA on

In this paper, the different "built in" material models based on the isotropic, kinematic and combined istropic-kinematic hardening theories available in Abaqus/Standard are evaluated for carbon steels. The results presented in this study are expected to provide important insight to practicing engineers dealing with inelastic material characteristics.