Submitted by luvsharma11 on

Hi all,

I am trying to model a solder joint in double lap shear. I am using the Modified Anand's Model. But for some reasons the analysis is not completing and does not gives any errors as well. Since I am new to abaqus, I am not able to solve this. Here is my input file:

---------------------------------------------------------------------------------------------------------------------------------------

 *Heading

** Job name: dl-3 Model name: Model-1

*Preprint, echo=NO, model=NO, history=NO, contact=NO

*Part, name=Part-1

*End Part

**  

**

** ASSEMBLY

**

*Assembly, name=Assembly

**  

*Instance, name=Part-1-1, part=Part-1

*Node

      1, -0.00700000022, 0.00700000022, 0.00700000022

      2, -0.00700000022, 0.00700000022,           0.

      3, -0.00700000022,           0.,           0.

      4, -0.00700000022,           0., 0.00700000022

      5,           0., 0.00700000022,           0.

      6,           0.,           0.,           0.

      7,           0.,           0., 0.00700000022

      8,           0., 0.00700000022, 0.00700000022

      9, -0.0399999991, -0.00600000005, 0.00700000022

     10, -0.0399999991, -0.00600000005,           0.

     11, -0.00700000022, -0.00600000005,           0.

     12, -0.00700000022, -0.00600000005, 0.00700000022

     13,           0., -0.00600000005,           0.

     14,           0., -0.00600000005, 0.00700000022

     15, -0.0399999991,           0.,           0.

     16, -0.0399999991,           0., 0.00700000022

     17, -0.00700000022, -0.0130000003,           0.

     18, -0.00700000022, -0.0130000003, 0.00700000022

     19,           0., -0.0130000003, 0.00700000022

     20,           0., -0.0130000003,           0.

     21, -0.00700000022, 0.0130000003, 0.00700000022

     22, -0.00700000022, 0.0130000003,           0.

     23, 0.0359999985, 0.00700000022, 0.00700000022

     24, 0.0359999985, 0.0130000003, 0.00700000022

     25, 0.0359999985, 0.0130000003,           0.

     26, 0.0359999985, 0.00700000022,           0.

     27, -0.00700000022, -0.0179999992,           0.

     28, -0.00700000022, -0.0179999992, 0.00700000022

     29, 0.0359999985, -0.0130000003,           0.

     30, 0.0359999985, -0.0179999992,           0.

     31, 0.0359999985, -0.0179999992, 0.00700000022

     32, 0.0359999985, -0.0130000003, 0.00700000022

     33, -0.0333999991, -0.00600000005,           0.

     34, -0.0267999992, -0.00600000005,           0.

     35, -0.0201999992, -0.00600000005,           0.

     36, -0.0136000002, -0.00600000005,           0.

     37, -0.0136000002, -0.00600000005, 0.00700000022

     38, -0.0201999992, -0.00600000005, 0.00700000022

     39, -0.0267999992, -0.00600000005, 0.00700000022

     40, -0.0333999991, -0.00600000005, 0.00700000022

     41, -0.0136000002,           0.,           0.

     42, -0.0201999992,           0.,           0.

     43, -0.0267999992,           0.,           0.

     44, -0.0333999991,           0.,           0.

     45, -0.0333999991,           0., 0.00700000022

     46, -0.0267999992,           0., 0.00700000022

     47, -0.0201999992,           0., 0.00700000022

     48, -0.0136000002,           0., 0.00700000022

     49, 0.000166666679, 0.0130000003,           0.

     50, 0.00733333314, 0.0130000003,           0.

     51, 0.0144999996, 0.0130000003,           0.

     52, 0.0216666665, 0.0130000003,           0.

     53, 0.0288333334, 0.0130000003,           0.

     54, 0.0287999995, 0.00700000022,           0.

     55, 0.0216000006, 0.00700000022,           0.

     56, 0.0143999998, 0.00700000022,           0.

     57, 0.00719999988, 0.00700000022,           0.

     58, 0.0288333334, 0.0130000003, 0.00700000022

     59, 0.0216666665, 0.0130000003, 0.00700000022

     60, 0.0144999996, 0.0130000003, 0.00700000022

     61, 0.00733333314, 0.0130000003, 0.00700000022

     62, 0.000166666679, 0.0130000003, 0.00700000022

     63, 0.00719999988, 0.00700000022, 0.00700000022

     64, 0.0143999998, 0.00700000022, 0.00700000022

     65, 0.0216000006, 0.00700000022, 0.00700000022

     66, 0.0287999995, 0.00700000022, 0.00700000022

     67, 0.000166666679, -0.0179999992, 0.00700000022

     68, 0.00733333314, -0.0179999992, 0.00700000022

     69, 0.0144999996, -0.0179999992, 0.00700000022

     70, 0.0216666665, -0.0179999992, 0.00700000022

     71, 0.0288333334, -0.0179999992, 0.00700000022

     72, 0.0287999995, -0.0130000003, 0.00700000022

     73, 0.0216000006, -0.0130000003, 0.00700000022

     74, 0.0143999998, -0.0130000003, 0.00700000022

     75, 0.00719999988, -0.0130000003, 0.00700000022

     76, 0.0288333334, -0.0179999992,           0.

     77, 0.0216666665, -0.0179999992,           0.

     78, 0.0144999996, -0.0179999992,           0.

     79, 0.00733333314, -0.0179999992,           0.

     80, 0.000166666679, -0.0179999992,           0.

     81, 0.00719999988, -0.0130000003,           0.

     82, 0.0143999998, -0.0130000003,           0.

     83, 0.0216000006, -0.0130000003,           0.

     84, 0.0287999995, -0.0130000003,           0.

     85,           0., 0.00350000011, 0.00700000022

     86,           0.,           0., 0.00350000011

     87,           0., 0.00350000011,           0.

     88,           0., 0.00700000022, 0.00350000011

     89, -0.00700000022, 0.00700000022, 0.00350000011

     90, -0.00700000022, 0.00350000011,           0.

     91, -0.00700000022,           0., 0.00350000011

     92, -0.00700000022, 0.00350000011, 0.00700000022

     93, -0.00350000011, 0.00700000022,           0.

     94, -0.00350000011, 0.00700000022, 0.00700000022

     95, -0.00350000011,           0.,           0.

     96, -0.00350000011,           0., 0.00700000022

     97, -0.0366999991,           0., 0.00700000022

     98, -0.0333999991,           0., 0.00350000011

     99, -0.0366999991,           0.,           0.

    100, -0.0399999991,           0., 0.00350000011

    101, -0.0399999991, -0.00600000005, 0.00350000011

    102, -0.0366999991, -0.00600000005,           0.

    103, -0.0333999991, -0.00600000005, 0.00350000011

    104, -0.0366999991, -0.00600000005, 0.00700000022

    105, -0.0399999991, -0.00300000003,           0.

    106, -0.0399999991, -0.00300000003, 0.00700000022

    107, -0.0333999991, -0.00300000003,           0.

    108, -0.0333999991, -0.00300000003, 0.00700000022

    109, -0.0300999992,           0., 0.00700000022

    110, -0.0267999992,           0., 0.00350000011

    111, -0.0300999992,           0.,           0.

    112, -0.0300999992, -0.00600000005,           0.

    113, -0.0267999992, -0.00600000005, 0.00350000011

    114, -0.0300999992, -0.00600000005, 0.00700000022

    115, -0.0267999992, -0.00300000003,           0.

    116, -0.0267999992, -0.00300000003, 0.00700000022

    117, -0.0234999992,           0., 0.00700000022

    118, -0.0201999992,           0., 0.00350000011

    119, -0.0234999992,           0.,           0.

    120, -0.0234999992, -0.00600000005,           0.

    121, -0.0201999992, -0.00600000005, 0.00350000011

    122, -0.0234999992, -0.00600000005, 0.00700000022

    123, -0.0201999992, -0.00300000003,           0.

    124, -0.0201999992, -0.00300000003, 0.00700000022

    125, -0.0168999992,           0., 0.00700000022

    126, -0.0136000002,           0., 0.00350000011

    127, -0.0168999992,           0.,           0.

    128, -0.0168999992, -0.00600000005,           0.

    129, -0.0136000002, -0.00600000005, 0.00350000011

    130, -0.0168999992, -0.00600000005, 0.00700000022

    131, -0.0136000002, -0.00300000003,           0.

    132, -0.0136000002, -0.00300000003, 0.00700000022

    133, -0.0103000002,           0., 0.00700000022

    134, -0.0103000002,           0.,           0.

    135, -0.0103000002, -0.00600000005,           0.

    136, -0.00700000022, -0.00600000005, 0.00350000011

    137, -0.0103000002, -0.00600000005, 0.00700000022

    138, -0.00700000022, -0.00300000003,           0.

    139, -0.00700000022, -0.00300000003, 0.00700000022

    140, -0.00350000011, -0.00600000005,           0.

    141,           0., -0.00600000005, 0.00350000011

    142, -0.00350000011, -0.00600000005, 0.00700000022

    143,           0., -0.00300000003,           0.

    144,           0., -0.00300000003, 0.00700000022

    145,           0., -0.00949999969,           0.

    146,           0., -0.00949999969, 0.00700000022

    147,           0., -0.0130000003, 0.00350000011

    148, -0.00700000022, -0.0130000003, 0.00350000011

    149, -0.00700000022, -0.00949999969, 0.00700000022

    150, -0.00700000022, -0.00949999969,           0.

    151, -0.00350000011, -0.0130000003, 0.00700000022

    152, -0.00350000011, -0.0130000003,           0.

    153,  8.33333397e-05, 0.00999999978,           0.

    154, 0.000166666679, 0.0130000003, 0.00350000011

    155,  8.33333397e-05, 0.00999999978, 0.00700000022

    156, -0.00700000022, 0.00999999978, 0.00700000022

    157, -0.00700000022, 0.0130000003, 0.00350000011

    158, -0.00700000022, 0.00999999978,           0.

    159, -0.00341666676, 0.0130000003, 0.00700000022

    160, -0.00341666676, 0.0130000003,           0.

    161, 0.00726666674, 0.00999999978,           0.

    162, 0.00733333314, 0.0130000003, 0.00350000011

    163, 0.00726666674, 0.00999999978, 0.00700000022

    164, 0.00719999988, 0.00700000022, 0.00350000011

    165, 0.00359999994, 0.00700000022, 0.00700000022

    166, 0.00359999994, 0.00700000022,           0.

    167, 0.00374999992, 0.0130000003, 0.00700000022

    168, 0.00374999992, 0.0130000003,           0.

    169, 0.0144499997, 0.00999999978,           0.

    170, 0.0144999996, 0.0130000003, 0.00350000011

    171, 0.0144499997, 0.00999999978, 0.00700000022

    172, 0.0143999998, 0.00700000022, 0.00350000011

    173, 0.0108000003, 0.00700000022, 0.00700000022

    174, 0.0108000003, 0.00700000022,           0.

    175, 0.0109166661, 0.0130000003, 0.00700000022

    176, 0.0109166661, 0.0130000003,           0.

    177, 0.0216333345, 0.00999999978,           0.

    178, 0.0216666665, 0.0130000003, 0.00350000011

    179, 0.0216333345, 0.00999999978, 0.00700000022

    180, 0.0216000006, 0.00700000022, 0.00350000011

    181, 0.0179999992, 0.00700000022, 0.00700000022

    182, 0.0179999992, 0.00700000022,           0.

    183,  0.018083334, 0.0130000003, 0.00700000022

    184,  0.018083334, 0.0130000003,           0.

    185, 0.0288166665, 0.00999999978,           0.

    186, 0.0288333334, 0.0130000003, 0.00350000011

    187, 0.0288166665, 0.00999999978, 0.00700000022

    188, 0.0287999995, 0.00700000022, 0.00350000011

    189,       0.0252, 0.00700000022, 0.00700000022

    190,       0.0252, 0.00700000022,           0.

    191,  0.025249999, 0.0130000003, 0.00700000022

    192,  0.025249999, 0.0130000003,           0.

    193, 0.0359999985, 0.00999999978,           0.

    194, 0.0359999985, 0.0130000003, 0.00350000011

    195, 0.0359999985, 0.00999999978, 0.00700000022

    196, 0.0359999985, 0.00700000022, 0.00350000011

    197, 0.0324000008, 0.00700000022, 0.00700000022

    198, 0.0324000008, 0.00700000022,           0.

    199, 0.0324166678, 0.0130000003, 0.00700000022

    200, 0.0324166678, 0.0130000003,           0.

    201,  8.33333397e-05, -0.0154999997, 0.00700000022

    202, 0.000166666679, -0.0179999992, 0.00350000011

    203,  8.33333397e-05, -0.0154999997,           0.

    204, -0.00700000022, -0.0154999997,           0.

    205, -0.00700000022, -0.0179999992, 0.00350000011

    206, -0.00700000022, -0.0154999997, 0.00700000022

    207, -0.00341666676, -0.0179999992,           0.

    208, -0.00341666676, -0.0179999992, 0.00700000022

    209, 0.00726666674, -0.0154999997, 0.00700000022

    210, 0.00733333314, -0.0179999992, 0.00350000011

    211, 0.00726666674, -0.0154999997,           0.

    212, 0.00719999988, -0.0130000003, 0.00350000011

    213, 0.00359999994, -0.0130000003,           0.

    214, 0.00359999994, -0.0130000003, 0.00700000022

    215, 0.00374999992, -0.0179999992,           0.

    216, 0.00374999992, -0.0179999992, 0.00700000022

    217, 0.0144499997, -0.0154999997, 0.00700000022

    218, 0.0144999996, -0.0179999992, 0.00350000011

    219, 0.0144499997, -0.0154999997,           0.

    220, 0.0143999998, -0.0130000003, 0.00350000011

    221, 0.0108000003, -0.0130000003,           0.

    222, 0.0108000003, -0.0130000003, 0.00700000022

    223, 0.0109166661, -0.0179999992,           0.

    224, 0.0109166661, -0.0179999992, 0.00700000022

    225, 0.0216333345, -0.0154999997, 0.00700000022

    226, 0.0216666665, -0.0179999992, 0.00350000011

    227, 0.0216333345, -0.0154999997,           0.

    228, 0.0216000006, -0.0130000003, 0.00350000011

    229, 0.0179999992, -0.0130000003,           0.

    230, 0.0179999992, -0.0130000003, 0.00700000022

    231,  0.018083334, -0.0179999992,           0.

    232,  0.018083334, -0.0179999992, 0.00700000022

    233, 0.0288166665, -0.0154999997, 0.00700000022

    234, 0.0288333334, -0.0179999992, 0.00350000011

    235, 0.0288166665, -0.0154999997,           0.

    236, 0.0287999995, -0.0130000003, 0.00350000011

    237,       0.0252, -0.0130000003,           0.

    238,       0.0252, -0.0130000003, 0.00700000022

    239,  0.025249999, -0.0179999992,           0.

    240,  0.025249999, -0.0179999992, 0.00700000022

    241, 0.0359999985, -0.0154999997, 0.00700000022

    242, 0.0359999985, -0.0179999992, 0.00350000011

    243, 0.0359999985, -0.0154999997,           0.

    244, 0.0359999985, -0.0130000003, 0.00350000011

    245, 0.0324000008, -0.0130000003,           0.

    246, 0.0324000008, -0.0130000003, 0.00700000022

    247, 0.0324166678, -0.0179999992,           0.

    248, 0.0324166678, -0.0179999992, 0.00700000022

*Element, type=C3D20R

1,  8,  5,  6,  7,  1,  2,  3,  4, 88, 87, 86, 85, 89, 90, 91,

   92, 94, 93, 95, 96

2,  16,  15,  44,  45,   9,  10,  33,  40, 100,  99,  98,  97, 101, 102, 103,

   104, 106, 105, 107, 108

3,  45,  44,  43,  46,  40,  33,  34,  39,  98, 111, 110, 109, 103, 112, 113,

   114, 108, 107, 115, 116

4,  46,  43,  42,  47,  39,  34,  35,  38, 110, 119, 118, 117, 113, 120, 121,

   122, 116, 115, 123, 124

5,  47,  42,  41,  48,  38,  35,  36,  37, 118, 127, 126, 125, 121, 128, 129,

   130, 124, 123, 131, 132

6,  48,  41,   3,   4,  37,  36,  11,  12, 126, 134,  91, 133, 129, 135, 136,

   137, 132, 131, 138, 139

7,   4,   3,   6,   7,  12,  11,  13,  14,  91,  95,  86,  96, 136, 140, 141,

   142, 139, 138, 143, 144

8,  20,  19,  14,  13,  17,  18,  12,  11, 147, 146, 141, 145, 148, 149, 136,

   150, 152, 151, 142, 140

 9,   5,   8,  62,  49,   2,   1,  21,  22,  88, 155, 154, 153,  89, 156, 157,

    158,  93,  94, 159, 160

10,  57,  63,  61,  50,   5,   8,  62,  49, 164, 163, 162, 161,  88, 155, 154,

    153, 166, 165, 167, 168

11,  56,  64,  60,  51,  57,  63,  61,  50, 172, 171, 170, 169, 164, 163, 162,

    161, 174, 173, 175, 176

12,  55,  65,  59,  52,  56,  64,  60,  51, 180, 179, 178, 177, 172, 171, 170,

    169, 182, 181, 183, 184

13,  54,  66,  58,  53,  55,  65,  59,  52, 188, 187, 186, 185, 180, 179, 178,

    177, 190, 189, 191, 192

14,  26,  23,  24,  25,  54,  66,  58,  53, 196, 195, 194, 193, 188, 187, 186,

    185, 198, 197, 199, 200

15,  19,  20,  80,  67,  18,  17,  27,  28, 147, 203, 202, 201, 148, 204, 205,

    206, 151, 152, 207, 208

16,  75,  81,  79,  68,  19,  20,  80,  67, 212, 211, 210, 209, 147, 203, 202,

    201, 214, 213, 215, 216

17,  74,  82,  78,  69,  75,  81,  79,  68, 220, 219, 218, 217, 212, 211, 210,

    209, 222, 221, 223, 224

18,  73,  83,  77,  70,  74,  82,  78,  69, 228, 227, 226, 225, 220, 219, 218,

    217, 230, 229, 231, 232

19,  72,  84,  76,  71,  73,  83,  77,  70, 236, 235, 234, 233, 228, 227, 226,

    225, 238, 237, 239, 240

20,  32,  29,  30,  31,  72,  84,  76,  71, 244, 243, 242, 241, 236, 235, 234,

    233, 246, 245, 247, 248

*Nset, nset=_PickedSet6, internal

   1,   2,   3,   4,   5,   6,   7,   8,  11,  12,  13,  14,  17,  18,  19,  20

  85,  86,  87,  88,  89,  90,  91,  92,  93,  94,  95,  96, 136, 140, 141, 142

 145, 146, 147, 148, 149, 150, 151, 152

*Elset, elset=_PickedSet6, internal

 1, 8

*Nset, nset=_PickedSet7, internal

   1,   2,   3,   4,   5,   6,   7,   8,   9,  10,  11,  12,  13,  14,  15,  16

  17,  18,  19,  20,  21,  22,  23,  24,  25,  26,  27,  28,  29,  30,  31,  32

  33,  34,  35,  36,  37,  38,  39,  40,  41,  42,  43,  44,  45,  46,  47,  48

  49,  50,  51,  52,  53,  54,  55,  56,  57,  58,  59,  60,  61,  62,  63,  64

  65,  66,  67,  68,  69,  70,  71,  72,  73,  74,  75,  76,  77,  78,  79,  80

  81,  82,  83,  84,  86,  88,  89,  91,  93,  94,  95,  96,  97,  98,  99, 100

 101, 102, 103, 104, 105, 106, 107, 108, 109, 110, 111, 112, 113, 114, 115, 116

 117, 118, 119, 120, 121, 122, 123, 124, 125, 126, 127, 128, 129, 130, 131, 132

 133, 134, 135, 136, 137, 138, 139, 140, 141, 142, 143, 144, 147, 148, 151, 152

 153, 154, 155, 156, 157, 158, 159, 160, 161, 162, 163, 164, 165, 166, 167, 168

 169, 170, 171, 172, 173, 174, 175, 176, 177, 178, 179, 180, 181, 182, 183, 184

 185, 186, 187, 188, 189, 190, 191, 192, 193, 194, 195, 196, 197, 198, 199, 200

 201, 202, 203, 204, 205, 206, 207, 208, 209, 210, 211, 212, 213, 214, 215, 216

 217, 218, 219, 220, 221, 222, 223, 224, 225, 226, 227, 228, 229, 230, 231, 232

 233, 234, 235, 236, 237, 238, 239, 240, 241, 242, 243, 244, 245, 246, 247, 248

*Elset, elset=_PickedSet7, internal

  2,  3,  4,  5,  6,  7,  9, 10, 11, 12, 13, 14, 15, 16, 17, 18

 19, 20

** Section: a

*Solid Section, elset=_PickedSet6, material=ABQ_CREEP_MOD_ANAND



** Section: c

*Solid Section, elset=_PickedSet7, material=Cu



*End Instance

**  

*Nset, nset=_PickedSet9, internal, instance=Part-1-1

  23,  24,  25,  26,  29,  30,  31,  32, 193, 194, 195, 196, 241, 242, 243, 244

*Elset, elset=_PickedSet9, internal, instance=Part-1-1

 14, 20

*Nset, nset=_PickedSet10, internal, instance=Part-1-1

   9,  10,  15,  16, 100, 101, 105, 106

*Elset, elset=_PickedSet10, internal, instance=Part-1-1

 2,

*Elset, elset=Set-1, instance=Part-1-1

 1,

*End Assembly

**

** MATERIALS

**

*Material, name=ABQ_CREEP_MOD_ANAND

** anand modified

*Creep, law=USER

**************************************************************************

** S1      Q/R      A      CSI     m      A0/H0      Shat         n

28.6E6 , 10278.43, 177016., 7.,   0.207, -90939.8E6, 52.4E6,     0.0177,

** a       T0      S2      S3    A1       A2        A3           A4

   1.6,     0., -0.0673E6, 0., 960.7E6, -0.956E6,  -3260581.8E6,24976815.5E6

*depvar

 1,

**************************************************************************

*Elastic

 4.8e+10, 0.36

*Material, name=Cu

** oxygen free

*Elastic

 1.14e+11, 0.31

**

** BOUNDARY CONDITIONS

**

** Name: BC-1 Type: Symmetry/Antisymmetry/Encastre

*Boundary

_PickedSet9, ENCASTRE

** ----------------------------------------------------------------

**

** STEP: analysis

**

*Step, name=analysis, nlgeom=YES, inc=10000

viscoplastic

*Visco, cetol=1e-06

0.1, 300., 2.31e-22, 1.

**

** BOUNDARY CONDITIONS

**

** Name: BC-2 Type: Displacement/Rotation

*Boundary

_PickedSet10, 1, 1, -0.0025

_PickedSet10, 2, 2

_PickedSet10, 3, 3

_PickedSet10, 4, 4

_PickedSet10, 5, 5

_PickedSet10, 6, 6

**

** OUTPUT REQUESTS

**

*Restart, write, frequency=0

**

** FIELD OUTPUT: F-Output-1

**

*Output, field

*Node Output

CF, RF, U

*Element Output, directions=YES

CE, CEEQ, CEMAG, E, LE, PE, PEEQ, PEMAG, S

*Contact Output

CDISP, CSTRESS

**

** HISTORY OUTPUT: H-Output-1

**

*Output, history

*Element Output, elset=Set-1

CE11, CE12, CE13, CE22, CE23, CE33, CEMAG, E11, E12, E13, E22, E23, E33, EP, INV3, MISES

PE11, PE12, PE13, PE22, PE23, PE33, PEMAG, PEP, PRESS, PS11, PS12, PS13, PS22, PS23, PS33, S11

S12, S13, S22, S23, S33, SP, TRESC, VE11, VE12, VE13, VE22, VE23, VE33, VS11, VS12, VS13

VS22, VS23, VS33

*End Step

----------------------------------------------------------------------------------------------------------------------------------------------------

Thanks.

Hi,

  I suppose your problem lies in STEP analysis. You can take some time in this. And could you tell me which version of ABAQUS you use?  

Sun, 03/18/2012 - 02:57 Permalink

can u share your modified anand model's vumat codes with me? I have studyed anand model for  a long time, but I cann't understand the corresponding theory. So if you can share the vumat or umat codes with me, I would appreciate it very much. my papers are as follows. if you have any ideas, I can also answer u. anyway, thanks you very much! 

[1] Haitao Wang, Huamin Zhou, Zhigao Huang, Yun Zhang, Xiaoxuan Zhao, Constitutive modeling of polycarbonate over a wide range of strain rates and temperatures, Mechanics of Time-Dependent Materials, (2016) 1-21.

[2] Haitao Wang, Huamin Zhou, Zhigao Huang, Yi Zhang, Haiyu Qiao, Zhipeng Yu, Experimental investigation and modeling of the mechanical behavior of PC/ABS during monotonic and cyclic loading, Polymer Testing, 50 (2016) 216-223.

[3] Haitao Wang, Yun Zhang, Zhigao Huang, Huang Gao, Yi Zhang, Xiping Gao, Huamin Zhou, Experimental and modeling study of the compressive behavior of PC/ABS at low, moderate and high strain rates, Polymer Testing, 56 (2016) 115-123.

[4] Haitao Wang, Yun Zhang, Huamin Zhou, Zhigao Huang, Constitutive modelling of polycarbonate at low, moderate and high strain rates, 2nd International Conference on Mechanical and Aeronautical Engineering, Hong Kong, 2016.

 

[5] Haitao Wang, Yun Zhang, Zhigao Huang, Zhongbin Tang, Yanpei Wang, Huamin Zhou, Establishment and comparison of four constitutive models of PC/ABS from low to high strain rates, Mechanics of Time-Dependent Materials, Under review.

Thu, 02/16/2017 - 03:12 Permalink

can u share your modified anand model's vumat codes with me? I have studyed anand model for  a long time, but I cann't understand the corresponding theory. So if you can share the vumat or umat codes with me, I would appreciate it very much. my papers are as follows. if you have any ideas, I can also answer u. anyway, thanks you very much! 

[1] Haitao Wang, Huamin Zhou, Zhigao Huang, Yun Zhang, Xiaoxuan Zhao, Constitutive modeling of polycarbonate over a wide range of strain rates and temperatures, Mechanics of Time-Dependent Materials, (2016) 1-21.

[2] Haitao Wang, Huamin Zhou, Zhigao Huang, Yi Zhang, Haiyu Qiao, Zhipeng Yu, Experimental investigation and modeling of the mechanical behavior of PC/ABS during monotonic and cyclic loading, Polymer Testing, 50 (2016) 216-223.

[3] Haitao Wang, Yun Zhang, Zhigao Huang, Huang Gao, Yi Zhang, Xiping Gao, Huamin Zhou, Experimental and modeling study of the compressive behavior of PC/ABS at low, moderate and high strain rates, Polymer Testing, 56 (2016) 115-123.

[4] Haitao Wang, Yun Zhang, Huamin Zhou, Zhigao Huang, Constitutive modelling of polycarbonate at low, moderate and high strain rates, 2nd International Conference on Mechanical and Aeronautical Engineering, Hong Kong, 2016.

 

[5] Haitao Wang, Yun Zhang, Zhigao Huang, Zhongbin Tang, Yanpei Wang, Huamin Zhou, Establishment and comparison of four constitutive models of PC/ABS from low to high strain rates, Mechanics of Time-Dependent Materials, Under review.

Thu, 02/16/2017 - 03:12 Permalink

can u share your modified anand model's vumat codes with me? I have studyed anand model for  a long time, but I cann't understand the corresponding theory. So if you can share the vumat or umat codes with me, I would appreciate it very much. my papers are as follows. if you have any ideas, I can also answer u. anyway, thanks you very much! 

[1] Haitao Wang, Huamin Zhou, Zhigao Huang, Yun Zhang, Xiaoxuan Zhao, Constitutive modeling of polycarbonate over a wide range of strain rates and temperatures, Mechanics of Time-Dependent Materials, (2016) 1-21.

[2] Haitao Wang, Huamin Zhou, Zhigao Huang, Yi Zhang, Haiyu Qiao, Zhipeng Yu, Experimental investigation and modeling of the mechanical behavior of PC/ABS during monotonic and cyclic loading, Polymer Testing, 50 (2016) 216-223.

[3] Haitao Wang, Yun Zhang, Zhigao Huang, Huang Gao, Yi Zhang, Xiping Gao, Huamin Zhou, Experimental and modeling study of the compressive behavior of PC/ABS at low, moderate and high strain rates, Polymer Testing, 56 (2016) 115-123.

[4] Haitao Wang, Yun Zhang, Huamin Zhou, Zhigao Huang, Constitutive modelling of polycarbonate at low, moderate and high strain rates, 2nd International Conference on Mechanical and Aeronautical Engineering, Hong Kong, 2016.

 

[5] Haitao Wang, Yun Zhang, Zhigao Huang, Zhongbin Tang, Yanpei Wang, Huamin Zhou, Establishment and comparison of four constitutive models of PC/ABS from low to high strain rates, Mechanics of Time-Dependent Materials, Under review.

Thu, 02/16/2017 - 03:12 Permalink

can u share your modified anand model's vumat codes with me? I have studyed anand model for  a long time, but I cann't understand the corresponding theory. So if you can share the vumat or umat codes with me, I would appreciate it very much. my papers are as follows. if you have any ideas, I can also answer u. anyway, thanks you very much! 

[1] Haitao Wang, Huamin Zhou, Zhigao Huang, Yun Zhang, Xiaoxuan Zhao, Constitutive modeling of polycarbonate over a wide range of strain rates and temperatures, Mechanics of Time-Dependent Materials, (2016) 1-21.

[2] Haitao Wang, Huamin Zhou, Zhigao Huang, Yi Zhang, Haiyu Qiao, Zhipeng Yu, Experimental investigation and modeling of the mechanical behavior of PC/ABS during monotonic and cyclic loading, Polymer Testing, 50 (2016) 216-223.

[3] Haitao Wang, Yun Zhang, Zhigao Huang, Huang Gao, Yi Zhang, Xiping Gao, Huamin Zhou, Experimental and modeling study of the compressive behavior of PC/ABS at low, moderate and high strain rates, Polymer Testing, 56 (2016) 115-123.

[4] Haitao Wang, Yun Zhang, Huamin Zhou, Zhigao Huang, Constitutive modelling of polycarbonate at low, moderate and high strain rates, 2nd International Conference on Mechanical and Aeronautical Engineering, Hong Kong, 2016.

 

[5] Haitao Wang, Yun Zhang, Zhigao Huang, Zhongbin Tang, Yanpei Wang, Huamin Zhou, Establishment and comparison of four constitutive models of PC/ABS from low to high strain rates, Mechanics of Time-Dependent Materials, Under review.

Thu, 02/16/2017 - 03:12 Permalink

can u share your modified anand model's vumat codes with me? I have studyed anand model for  a long time, but I cann't understand the corresponding theory. So if you can share the vumat or umat codes with me, I would appreciate it very much. my papers are as follows. if you have any ideas, I can also answer u. anyway, thanks you very much! 

[1] Haitao Wang, Huamin Zhou, Zhigao Huang, Yun Zhang, Xiaoxuan Zhao, Constitutive modeling of polycarbonate over a wide range of strain rates and temperatures, Mechanics of Time-Dependent Materials, (2016) 1-21.

[2] Haitao Wang, Huamin Zhou, Zhigao Huang, Yi Zhang, Haiyu Qiao, Zhipeng Yu, Experimental investigation and modeling of the mechanical behavior of PC/ABS during monotonic and cyclic loading, Polymer Testing, 50 (2016) 216-223.

[3] Haitao Wang, Yun Zhang, Zhigao Huang, Huang Gao, Yi Zhang, Xiping Gao, Huamin Zhou, Experimental and modeling study of the compressive behavior of PC/ABS at low, moderate and high strain rates, Polymer Testing, 56 (2016) 115-123.

[4] Haitao Wang, Yun Zhang, Huamin Zhou, Zhigao Huang, Constitutive modelling of polycarbonate at low, moderate and high strain rates, 2nd International Conference on Mechanical and Aeronautical Engineering, Hong Kong, 2016.

 

[5] Haitao Wang, Yun Zhang, Zhigao Huang, Zhongbin Tang, Yanpei Wang, Huamin Zhou, Establishment and comparison of four constitutive models of PC/ABS from low to high strain rates, Mechanics of Time-Dependent Materials, Under review.

Thu, 02/16/2017 - 03:12 Permalink