Harnessing snap-through instability in soft dielectrics to achieve giant voltage-triggered deformation
Submitted by Christoph Keplinger on Fri, 2011-10-28 17:54.For a dielectric elastomer membrane we show giant voltage-triggered expansion of area by 1692%, far beyond the largest values reported in the literature.