Shear-lag model

Kmomeni's picture

Carbon Nanohorn Reinforced Nanocomposites...

I have formulated a shear-lag model for calculating the variation of stress along carbon nanohorns (CNHs), which are conical shaped wrapped carbon sheets, embedded in an epoxy matrix under axial loading.  I found that the stress distribution along the length of CNHs depends on the cone angle of these structures and maximum normal axial stress has a smaller value in CNHs compared to a carbon nanotube (CNT) with same cross-section as of the CNH's tip.  Furthermore, I read an article stating that synthesis of CNHs are easier compared to CNTs.  However, the only article I could find which has s