Effect of mechanical pre-stretch on the stabilization of dielectric elastomer actuation

A dielectric elastomer is capable of giant electromechanical actuation but fails at breakdown due to instability under certain conditions with a small deformation. By applying a mechanical pre-stretch, one obtains a stabilized large actuation.