Journal Club Theme of January 2007: Biomechanics and Non-Affine Kinematics
Submitted by MichelleLOyen on Mon, 2007-01-08 17:53.Biological materials are frequently constructed of hydrated biopolymer networks. Examples include fibrous collagen in the extracellular matrix and actin within the cell's cytoskeleton. There are differences in the molecular composition of the biopolymer subunits as well as differences in the network density and organization. Images can be seen here and here for dense collagen networks and for portions of actin networks look at images here and here.
»