Composite tape spring hinge

Jinxiong Zhou's picture

Optimizing deployment dynamics of composite tape-spring hinges

The composite tape-spring hinge (CTSH) is a lightweight structural connector widely employed in space structures, including spacecraft and satellites, due to its high specific strength and stiffness. Introducing cutouts enables CTSH to possess folding and deployment capability, while optimizing the cutouts finely to optimize the performance of CTSH. However, the interaction between cutout size and the dynamic deployment of CTSH is a novel topic.