Universal Displacements in Inextensible Fiber-Reinforced Linear Elastic Solids

For a given class of materials, universal displacements are those displacements that can be maintained for any member of the class by applying only boundary tractions. In this paper we study universal displacements in compressible anisotropic linear elastic solids reinforced by a family of inextensible fibers. For each symmetry class and for a uniform distribution of straight fibers respecting the corresponding symmetry we characterize the respective universal displacements. A goal of this paper is to investigate how an internal constraint affects the set of universal displacements.