User login

Navigation

You are here

open cell foam

Cutting iron foam samples

Hi, I have a sheet of open cell pure iron foam (porosity> 90% , thickness around 2.5 mm), and I would like to prepare 1 cm x 1 cm samples for subsequent compression tests. My foam is ductile and also it can be easily squeezed or bended with hand. I was wondering if I use a big rotatory saw (Bosch 4310, picture attached) to cut long rectangular strips (cuboids) of the foam (20 cm x 1 cm), could it significantly change the mechanical properties of the whole foam sheet, or it would change the mechanical properties of the cutting surface only.